Products
Medium-MFR PFA
  • Medium-MFR PFAMedium-MFR PFA

Medium-MFR PFA

Zhongwang, trusted Chinese supplier for bulk sourcing Medium-MFR PFA, supplies balanced-performance perfluoroalkoxy (PFA) fluoropolymer pellets (MFR 6-15 g/10 min, measured 372 ℃/5 kg, ASTM D1238) for global B2B fine-chemical, semiconductor fluid component, precision-injection-molding and wire-cable extrusion purchasers. Our Medium-MFR PFA strikes an optimal balance between melt-strength, stress-crack resistance and melt-flowability. It retains full PFA intrinsic merits: universal chemical inertness, continuous service temperature-200 ℃ ~ 260 ℃, outstanding dielectric performance, UL94 V-0 flame retardancy. Suitable for precision-injection fittings, thin-to-medium-wall tubing, wire-cable insulation, semiconductor-grade fluid parts and medium-thickness corrosion-resistant components.

    Located in Yuyao China Plastics City, Zhongwang provides diversified Medium-MFR PFA grades for worldwide industrial buyers. PFA (Perfluoroalkoxy) is melt-processable perfluorinated copolymer of tetrafluoroethylene and perfluoro-alkyl-vinyl ether. Medium MFR PFA is intermediate- molecular- weight PFA resin, sitting between low-MFR high-melt-strength grades and high-MFR high-flow grades. Compared with low-MFR PFA, medium-MFR PFA delivers better melt-flow for intricate-cavity filling, while compared with high-MFR PFA, it maintains superior melt-strength and environmental-stress-crack-resistance (ESCR) for pressure-bearing parts. Many purchasers blindly select low-MFR PFA for precision-thin-wall injection and encounter incomplete filling, or adopt high-MFR PFA for pressure-bearing tubing leading to higher stress-cracking risk.

    Our medium-MFR-series PFA includes general-purpose medium-MFR injection-molding grade, wire-cable extrusion grade and semiconductor-suitable medium-purity grade. According to customers’ target MFR value, processing-technology (injection / extrusion / transfer-molding), wall-thickness, pressure-bearing requirement, chemical-medium environment and metal-ion-extractables-specification, our technical team selects suitable Medium-MFR PFA grades for mass-production projects. Modified anti-static and filled variants are available upon special request. Note: Medium MFR PFA offers balanced comprehensive performance; for ultra- thick- wall heavy- pressure lining please choose low- MFR PFA; for ultra- thin- wall high- speed multi- cavity parts please consider high- MFR PFA.

    Medium MFR PFA


    What is Medium MFR PFA

    Medium MFR PFA is intermediate-molecular-weight perfluoroalkoxy fluoropolymer resin with MFR 6-15 g/10 min (372 ℃ /5 kg, ASTM D1238). Its molecular-weight is between low-MFR and high-MFR PFA, achieving trade-off of melt-strength, anti-stress-crack property and melt-flowability. It inherits all core advantages of perfluoropolymer: excellent resistance to nearly all strong acids, alkalis and organic solvents; continuous service-temperature-200 ℃ ~ 260 ℃; excellent high-frequency electrical insulation; limiting-oxygen-index 95 %, UL94 V-0 non-flammable performance.

    Medium MFR PFA can be processed by injection-molding, extrusion, transfer-molding and compression-molding; typical barrel-temperature 340-380 ℃, die-temperature 360-395 ℃. Even raw-material meets specification, defects such as short-shot, weld-line weakness, surface melt-fracture will appear if temperature-profile, back-pressure or screw-L/D design is unreasonable. Processors must strictly control thermal-history; prolonged residence above 390 ℃ will trigger fluoropolymer molecular-chain degradation, mechanical-property loss and corrosive-gas release. For semiconductor fluid-path components, medium-purity or ultra-high-purity medium-MFR PFA shall be selected to guarantee ultra-low-metal-ion-extractables.


    Main Grade Categories & Core Performance Advantages

    Our Medium MFR PFA product line is divided into three mainstream series according to processing characteristics: medium-MFR injection-molding Medium MFR PFA, wire-cable-extrusion Medium MFR PFA, medium-purity semiconductor-fluid Medium MFR PFA.

    1.  Medium- MFR Injection- Molding Medium MFR PFA Medium-MFR injection-molding PFA, MFR 6-15 g/10 min, balanced melt-flow and moderate melt-strength. Good filling for medium-thin-wall intricate fluoroplastic fittings, valve inserts, pump impeller housings. Main applications: fine-chemical corrosion-resistant injection fittings, instrument-valve internal components, general-semiconductor fluid-path injection parts, sample-cell housings.

    2.  Wire- Cable- Extrusion Medium MFR PFA Wire-cable-extrusion PFA, MFR 6-12 g/10 min, stable extrusion melt-homogeneity, balanced tensile-elongation and flex-life. Main applications: medium-speed high-temperature wire-cable primary-insulation, multi-core cable jacketing, small-diameter chemical-instrument PFA tubing extrusion.

    3.  Medium- Purity Semiconductor- Fluid Medium MFR PFA Medium-purity medium-MFR PFA, controlled low-impurity-end-groups, strictly-restricted metal-ion-extractables. Main applications: non-ultra-critical semiconductor wet-process fluid components, fine-pharmacy corrosion-resistant fluid-pipe fittings, analytical-instrument flow-cell parts.


    Technical Specifications

    Item

    Reference Data

    Product

    Medium-MFR PFA / Intermediate-Molecular-Weight Perfluoroalkoxy Fluoropolymer Pellets

    Brand

    Zhongwang

    Melt Flow Rate

    MFR 6-15 g/10 min (372 ℃, 5 kg, ASTM D1238), grade-dependent

    Density

    2.12-2.17 g/cm³ (ASTM D792)

    Melting Point

    300-310 ℃ (ASTM D4591)

    Tensile Strength

    ≥30 MPa typical value (ASTM D638)

    Elongation at Break

    ≥280 % typical value (ASTM D638)

    Continuous Service Temperature

    -200 ℃ ~ 260 ℃, short-term peak 270 ℃

    Limiting Oxygen Index

    95 % (ASTM D2863)

    Flammability

    UL94 V-0 (1.5 mm thickness)

    Dielectric Constant (1 MHz)

    2.15 (ASTM D150)

    Appearance

    Translucent ivory-white cylindrical pellets

    Processing Method

    Injection-Molding, Extrusion, Transfer-Molding, Compression-Molding

    Standard Packaging

    25 kg moisture-proof PE inner-bag + hard-paper drum packaging

    Place of Origin

    Yuyao, Zhejiang, China

    Available Documents

    COA, TDS, MSDS, mechanical-performance test report, RoHS / REACH statement

    Note: All listed figures are typical reference values. Real parameters shall refer to batch-specific COA and test certificates. Medium-MFR PFA provides balanced comprehensive performance; ultra-heavy-wall high-pressure lining applications should adopt low-MFR PFA. Avoid prolonged material residence above 390 ℃ to prevent fluoropolymer thermal-degradation and corrosive-gas release.


    Application & Grade Selection Guidance

    Selecting Medium MFR PFA cannot judge only by MFR value. Buyers need to evaluate processing-technology, finished-part wall-thickness, pressure-bearing requirement, chemical-medium contact environment, flex-fatigue condition and purity-level demand.

    - Medium- MFR Injection- Molding Medium MFR PFA: Recommended for fine-chemical corrosion-resistant injection fittings, instrument-valve inserts, general-semiconductor fluid-path injection components, sample-cell housings. - Wire- Cable- Extrusion Medium MFR PFA: Prioritize for medium-speed high-temperature wire-cable insulation, multi-core cable jacketing, small-diameter chemical-instrument PFA tubing. - Medium- Purity Semiconductor- Fluid Medium MFR PFA: Suitable for non-ultra-critical semiconductor wet-process fluid-parts, fine-pharmacy corrosion-resistant pipe-fittings, analytical-instrument flow-cell housings.

    When sending inquiry, please inform our team of target MFR range, processing-technology, finished-part wall-thickness, pressure-bearing requirement, chemical-medium type and purity-specification. Our technical team will recommend matched medium MFR PFA grades. Small-batch trial-production before mass-order is highly suggested; pay attention to testing environmental-stress-crack-resistance and weld-line mechanical-performance.


    Compliance & Quality Assurance

    Our Medium MFR PFA adopts virgin perfluoroalkoxy fluoropolymer raw-material; recycled-material mixing is strictly forbidden for fluoropolymer batches. Every batch completes MFR test, density inspection, melting-point verification and mechanical-property detection before shipment. Raw-material sources maintain long-term cooperation with well-known domestic and international fluoropolymer manufacturers.

    We support third-party mechanical and chemical-resistance inspection appointed by purchasers. Repeated thermal-cycles will cause fluoropolymer molecular-chain scission, leading to drop of tensile strength, elongation and stress-crack-resistance performance; regrind reuse is strongly not encouraged for PFA components under pressure-bearing or corrosion-service condition. We can supply COA, TDS, MSDS and corresponding performance-test reports, together with RoHS / REACH compliance statement according to project requirements.


    Our Supply Strength

    Zhongwang is located in Yuyao China Plastics City International Business Center, China’s largest plastic-raw-material trading hub. Geographically, it sits 60 km away from Beilun Port and 80 km away from Hangzhou Xiaoshan International Airport, enjoying convenient land-sea-air comprehensive logistics conditions.

    Apart from Medium MFR PFA, our product portfolio covers PP, PE, ABS, PC, PC/ABS, PA, EVA, TPV and other polymer materials, covering fine-chemical-equipment, semiconductor-auxiliary, automotive, home appliance, electronic-electrical and daily-commodity industries. We keep stable long-term partnerships with domestic & international resin suppliers. Apart from spot stock supply and local delivery service, our technical group can provide material-selection consultation, process docking and full-set application technical support for customer projects.


    Processing Guidance & Common Pitfalls

    Even purchasing qualified Medium MFR PFA, improper molding/extrusion operations will trigger short-shot, internal voids, weak weld-lines, melt-fracture and premature-part-failure. We summarize typical mistakes collected from cooperative fluoroplastic processing factories:

    1.  Improper processing- temperature setting. Medium MFR PFA requires barrel-temperature 340-380 ℃, die-temperature 360-395 ℃. Too-low melt-temperature will cause incomplete filling, poor melt-fusion and weak weld-lines. Do not directly copy processing parameters of low-MFR PFA or high-MFR PFA grades.

    2.  Excessive material residence- time inside barrel. Strictly avoid residence time longer than 15-20 min above 380 ℃; temperature exceeding 390 ℃ will cause fluoropolymer thermal-degradation, releasing corrosive fluorine-containing gas and permanently degrading mechanical performance. Machine shutdown procedure shall follow fluoropolymer standard-operation-specification.

    3.  Unscrew equipment selection. Medium-MFR PFA still belongs to high-viscosity fluoropolymer, requiring fluoropolymer-special screw with L/D 24-30, compression-ratio 2-3:1. Ordinary general-plastic screw will lead to insufficient plasticizing and unstable melt-output.

    4.  Mis- application for extreme- working- condition parts. For ultra-thick-wall heavy-pressure tank-lining parts, select low-MFR PFA for higher melt-strength and anti-stress-crack performance. For ultra-thin-wall multi-cavity high-speed-injection-parts, select high-MFR PFA for better flow-ability.

    5.  Neglecting post- molding annealing treatment. Medium-thickness PFA parts retain internal residual-stress; appropriate annealing helps release residual-stress and improves environmental-stress-crack-resistance in corrosive-medium service.

    Before switching production to medium MFR PFA, thoroughly purge and clean extruder / injection-machine barrel and screw to eliminate residual non-fluoropolymer plastic materials.


    Packing & Shipment

    Medium MFR PFA uses PE inner-bag plus 25 kg hard-paper-drum packaging. Pellets shall be stored in cool dry warehouse, avoid direct sunlight and high-heat source during storage and transit. Goods are stacked on standard plastic pallets to prevent dampness and mechanical damage in sea or land transportation. We support multiple trade terms such as FOB Ningbo, CIF. Spot goods can be delivered quickly after PO confirmation. For large-tonnage long-term framework orders, we coordinate stable allocation from fluoropolymer manufacturers. Real-shot photos of packing and container-loading can be provided upon buyer’s request.


    FAQ

    Q1: What is Medium MFR PFA? What is the main practical difference compared with low- MFR / high- MFR PFA? 

    A1: Medium MFR PFA is intermediate-molecular-weight perfluoroalkoxy fluoropolymer resin with MFR 6-15 g/10 min (372 ℃/5 kg). It balances melt-flow-ability and melt-strength. Low-MFR PFA (0.8-6 g/10 min) owns higher-melt-strength and superior-stress-crack-resistance for ultra-thick-wall heavy-pressure-lining parts. High-MFR PFA (>15 g/10 min) provides better-flow-ability for ultra-thin-wall intricate-parts, but melt-strength and stress-crack-resistance decline. Medium-MFR PFA is the universal work-horse grade for medium-wall precision-components, tubing and wire-cable extrusion.

    Q2: Does Medium MFR PFA need drying before processing? 

    A2: PFA has extremely low-moisture-absorption property. Under normal cool-dry sealed-storage, pre-drying is not required. If pellets absorb moisture due to damp-environment storage, dry at 120-150 ℃ for 4-6 hours. Do not adopt excessive high-temperature drying.

    Q3: Can you offer Medium MFR PFA samples for lab test and trial- production? 

    A3: Yes, small-quantity samples are available for customer testing purposes. Sample freight will be discussed separately. Notice: fluoropolymer processing window is narrow; actual trial-verification on target equipment is essential.

    Q4: What documents can you provide for purchase and export of medium MFR PFA? 

    A4: We can provide COA, TDS, MSDS, mechanical-performance test report and RoHS / REACH compliance statement according to project requirements. Corrosion-resistance performance needs to be verified under customer-specific actual chemical-medium condition.

    Q5: Can I add PFA regrind scraps for mass- production parts? 

    A5: PFA molecular-chain will degrade after thermal-history. For pressure-bearing, corrosion-resistant industrial PFA finished-parts, adding regrind is strongly not recommended. If non-critical static parts need to use regrind, full-performance retest must be completed.

    Send Inquiry
    Contact Info
    • Address

      Building 1, China Plastics International Business Center, No. 285 Shunda West Road, Yuyao City, Ningbo City, Zhejiang Province, China

    If you have any enquiry about quotation or cooperation, please feel free to email us or use the following inquiry form.Our sales representative will contact you within 24 hours. Thank you for your interest in our products.

    X
    We use cookies to offer you a better browsing experience, analyze site traffic and personalize content. By using this site, you agree to our use of cookies. Privacy Policy
    RejectAccept